Polyester woven in Black/White, 140 cm wide and 250 g/m², made from 3 % elastane, 5 % polyamide, 17 % polyester and 75 % viscose. Sold by the metre.

0.5 m cost €8.45

from 0.2 m, in steps of 0.1 m

Your legal guarantee rights

in stock

Delivery time approx. 3–5 working days

Free shipping within Germany from €50

Fabric type
Woven
Material
3 % Elasthan, 5 % Polyamide, 17 % Polyester, 75 % Viskose
Width
approx. 140 cm
Weight
approx. 250 g/m²
Colour
Schwarz/Weiß
Pattern
Karo
Care
  • Wash at 30°CWash at 30°C
  • Do not ironDo not iron
  • Wash without fabric softener or bleachWash without fabric softener or bleach
  • Do not tumble dryDo not tumble dry
Muster
Karo
Gewicht
250 g/m²
Breite
140 cm

Description

This polyester fabric keeps its colour and its shape even when it goes into the machine regularly. Weight per square metre comes to 250 g/m², width to 140 cm. It is woven from 3 % elastane, 5 % polyamide, 17 % polyester and 75 % viscose.

In Black/White the fabric reads clear and severe. For clothing meant to look matter-of-fact it is the first choice. Checks are a classic pattern that can read sporty or elegant — the cut decides. The fabric slips while cutting. With clips instead of pins and a rotary cutter the layer stays where it belongs.

What Bengaline schwarz-weiß kariert is suitable for

  • blouses and tunics
  • scarves and wraps
  • occasion wear

Care instructions:

Frequently asked questions

Which needle do I take?

A fine universal or microtex needle. The thinner the fabric, the finer the needle: too strong a needle leaves visible holes that never close again.

Scissors or rotary cutter?

On slippery goods the rotary cutter, because it does not lift the fabric. Scissors drag the layer along and the edge is no longer true.

Why does the seam pucker?

Because needle and stitch length do not suit the fabric. A fine needle, a shorter stitch and less presser foot pressure solve most of it. On very thin goods tissue paper under the seam helps, torn away afterwards.

What ironing temperature?

Moderate, and from the reverse. Viscose and polyester do not take the heat used for cotton; too hot and the surface turns shiny or melts.

Cookies and privacy

We need necessary cookies for the cart, sign-in and this choice. With your consent, our server sends details of your visit (products viewed, cart, purchases, IP address, browser) to Meta (Facebook, Instagram) to measure our ads – including to the USA. You can change this at any time under “Cookie settings”. More in our privacy policy.